Emralon GP 1904
Use an external-atomizing spray gun with 35-50 psi air pressure and adjust the gun to give a well-atomized spray.
For optimum performance, the final coating thickness should be 0.0003-0.0010 inches (0.008 to 0.025 millimeters).
When properly applied, the coating will be even and free of runs, blisters, or "fish eyes."
Some electrostatic spray systems may be used to apply Emralon GP 1904.
Call Acheson's Technical Finishes Department for details, (800) 255-1908.
Emralon GP 1904 can also be applied by dipping.
The product should be diluted 3:2 (product:solvent) by weight with MEK.
The average dip coating will produce a heavier coat, but a precure of ten minutes at 250' to 275'F (121' to 135'C) or one minute at 350'F (177'C) is required between dips. Dip-spin will require two or three coats.
A partial cure of one minute at 350'F (177'C) is required between coats.
Á¦Ç°°ü·ÃºÐ¾ß ±âŸ
Acheson Colloids Co.
ÀüÈ­¹øÈ£ 810-984-5581,800-255-1908
Æѽº¹øÈ£ 810-984-1446
ȨÆäÀÌÁö www.achesonindustries.com
À̸ÞÀÏ web.mail@nstarch.com
ÁÖ¼Ò 1600 Washington Avenue Port Huron, MI 48060 USA
ÀÌÁ¦Ç°¿¡ ´ëÇØ µî·ÏµÈ ÆǸž÷ü°¡ ¾ø½À´Ï´Ù.