WM 80 L
The WM 80 L anodizing process is a modification of conventional sulfuric acid anodizing. WM 80 L protects the newly formed anodic coating from the electrolyte during the anodizing process, increasing the efficiency of the coating formation.
Harder coatings at temperatures 77'F - 86'F (25'C-30'C) are achieved compared to conventional sulfuric acid anodizing at temperatures above 77'F(25'C).